Abstract of the talk by Patrick Swolona:

 

Progress Through Retraction: Rethinking Contact Angles to Probe Surface Activation and Joint Performance

 

Contact angle measurement has long been used to judge whether a surface is ready for bonding. It is used to assess the surface condition, for example after plasma, corona or flame treatment or cleaning. Although static contact angles are widely used, the receding contact angle is more sensitive to contamination and incomplete activation, which are decisive for adhesion. Dynamic measurements are rarely used because they are complex and time-consuming. We introduced the Stood-up Drop (SUD) technique to solve this problem. With this technique, it is possible to determine the receded contact angle within seconds instead of hours. By initially spreading a water drop into a thin film and subsequently allowing capillary forces to retract it into a stable “stood-up” configuration (see figure 1), the method ensures that the measured angle reflects a dewetting state, as recently demonstrated in Soft Matter (2026)1.

 

In this contribution, we summarize two years of applied laboratory work and customer-driven studies highlighting the method’s broad relevance. Representative examples include adhesion prediction for pressure sensitive adhesives and PU based glues, optimisation of plasma and flame treatments as well as cleanliness evaluation prior to bonding. In correlations with reference tests like peel strength or lap-shear strength measurements for adhesive joints, the receding contact angle accessed via the SUD proved markedly more sensitive with wider discrimination scales and reduced scatter compared to advanced or static angles.

 

Talk

Progress Through Retraction: Rethinking Contact Angles to Probe Surface Activation and Joint Performance

Patrick Swolona

Application Market Manager, KRÜSS GmbH