Sample holders and preparation sets for analyzing solids

SH0910 – Aluminum sample holder for contact angle measurements on powders and pigments

  • Bookmark

We have developed the SH0910 aluminum sample holder for measuring the contact angle on powders and pigments using the Washburn method. The easy to clean sample tube with a perforated base is to be equipped with a filter paper base, filled with the sample and the holder, within seconds, hung in the respective force sensor adaptor. The matching filter paper SH0711 is available from us in sets of 100 filters.