Dynamic Foam Analyzer
Produktvergleich
General specifications
Temperature measurement
Sensor
PT100
Range
4 to 90 °C
Resolution
0.1 °C
Precision
±0.1 °C
Accuracy
1/3 DIN B (±0.1 °C at 0 °C / ±0.8 °C at 400 °C)
Locations
inside sample liquid
External sensor
optional
Zubehör
Glass columns
20 and 40 mm diameter, temperature control option
Filter plates for sparging
diameter: 14 and 30 mm
Filter plate porosities
G1: nominal maximum pore size: 100 to 160 μm
G2: nominal maximum pore size: 40 to 100 μm
G3: nominal maximum pore size: 16 to 40 μm
G4: nominal maximum pore size: 10 to 16 μm
Material of columns and frits
borosilicate glass (norm: ISO 4793)
Material of sealings
silicone and FKM
Sample dimensions
Min. recommended sample volume
50 mL with 40 mm diameter column
20 mL with 20 mm diameter column
Instrument dimensions
Footprint
245 mm × 275 mm (W × D)
Height
460 mm
Weight (without accessories)
9 kg
Environment
Operating temperature
15 to 30 °C
Humidity
without condensation
Interfaces
PC
1× USB 2.0
Power supply
Voltage
100 to 240 V
Power consumption
30 W
Frequency
50 to 60 Hz
Temperature control
Type of temperature control
optional: double-walled glass column
Range of temperature control
4 to 90 °C
(additional thermostat needed)
Measurement specifications
Software
Software type
ADVANCE
Software languages
Chinese (simplified), English, French, German, Japanese, Korean, Portuguese, Russian, Spanish
Software modules
Foam analysis (recommended)
Remote Control API (optional)
Measurement specifications
Analyzed foam characteristic
foamability and foam stability
Results
foam height
liquid height
total height
foam capacity
maximum foam density
expansion rate
foam half life time
drainage half life time
sample temperature
Product group specifications
Illumination
Types
LED
Wave length, dominant (height detection)
469 nm (optional IR: 850 nm)
Camera system
Diameter of minimum detectable bubble
-
Mean field of view size
-
Focus
-
Electrodes
Material
-
Highest sensor position
-
Measured entity
-
Theoretical measurement range
-
Operating system
Internal gas flow rate
0.2 to 1 L/min
External gas flow rate
0.05 to 1 L/min
Approved gases
air
nitrogen
carbon dioxide
Approved pressure
5 ± 0.5 bar
Approved temperature
4 to 90 °C
Stirring speed
up to 8000 rpm
Camera system (standard)
Connection
-
Performance
-
Line sensor
Sensor resolution
1728×1px
Spatial resolution
200 dpi | 0.125 mm
Temporal resolution
20 fps
Scanning length
216 mm