Sample holders

ST10 – Set for measuring contact angle in bulk liquid

  • Bookmark

We have developed the sample holder and dosing set ST10 for measuring contact angle in a bulk liquid phase. Gas bubbles (Captive Bubble) or drops are dosed beneath the sample with the help of the set’s special needle and cuvette, e.g. for analyzing hydrogels and highly energetic and structured surfaces. The special holders optimize measurements on contact lenses, films and textiles as well as on rigid samples.